Structures for the Mounting FV Panels
(IPSSTAL)

 

The profiles better express theirs advantages compared with the building traditional materials, like steel, so far used in a lot of installations.
Thanks to high quality materials are able to resist from the cold of the winter season, to the hot of the summer season, avoiding the risk of wear and tear due to the corrosion
.

 


 
Structures Features
 
Mechanical Features

 

• More reduced weight of the structures

High resistance to corrosion thanks to anodization  thickness 13-15 μm of the profiles surface and the  tendency of the material to passivate in the air

High strenght reported to weight, obtained thanks to  an attentive study of the profiles turned to the optimisation of the mass in function of the maximum  of strenght

Easy realization of the structures thanks to the large  range of accessories studied on purpose of solar panels installations and the absolute compatibility with all the accessories on ALUSIC catalogue

Aesthetics impact reduced to minimum

Absolutely diamagnetic of the materia

Easily recycling of the material turn to safeguard the  environment also in case of dismantling of the  structures

The mechanical characteristics obtained after heat treatment :

Alloy 6060:

- Maximum Stress: 215 N/ mm2

- Yeld Stress: 160 N/ mm2

- Extension: 12%

- Handness: 70 HB

Alloy 6063:

- Maximum Stress: 245 N/ mm2

- Yeld Stress: 200 N/ mm2

- Extension: 9%

- Handness: 80 HB


Technical Data

 

Extruded aluminium profiles are realized in primary aluminium alloy EN AW-6060 (AlMgSi 0.5) – EN  AW6063 (AlMgSi1

The metallurgic state of supplied bars is T6  (solution heat treatment and artificially aged

Chemical composition Alloy 6060:

- Cu: 0.10

- Fe: 0.1-0.3

-Mn: 0.10

- Mg: 0.35-0.6

- Si: 0.3-0.6

- Zn: 0.15

- Cr: 0.05

- Ti: 0.10

- Al: Resto

Chemical composition Alloy 6063:

- Cu: 0.10

- Fe: 0.35

-Mn: 0.10

- Mg: 0.45-0.9

- Si: 0.2-0.6

- Zn: 0.10

- Cr: 0.10

- Ti: 0.10

- Al: Resto

 



Other Features

 

Young Modulus: 69000 N/mm2

Electric Resistively: 0.033
Ωmm2/m

Thermal Conductivity: 210 W/mK

Casting Temperature: 615-655 °C

Coefficient of Thermal Expansion: 25x10-6 K-1




 